Profiled steel, plastisol and aluminium roofs

Metal roof coating and refurbishment

Yes, where the sheeting still has structural capacity and corrosion is at the surface rather than through the sheet. A metal roof coating system cleans and prepares the profile, treats cut edges and fixings, and bonds a seamless liquid rubber membrane to the steel. It interrupts the corrosion cycle, seals every lap and fastener in one layer, and avoids stripping the roof.

01254 433987

What fails, and why

Investigate the cause before specifying repairs or a coating.

Cut edge corrosion spreading along the eaves

Once the protective coating is broken at a cut edge, corrosion creeps back under it. Cleaning and treating that edge before coating is what stops it continuing.

Leaking fastener heads

Hundreds of fixings penetrate the sheet. Each perished washer is a leak path, and they are sealed by the membrane rather than individually patched.

Coatings that peel after two winters

Almost always an adhesion problem: contamination left in place, no primer, or a coating applied over a chalked factory finish without preparation.

Fragile and ageing sheets

Old profiled sheets and rooflights may not be safe to walk on. Fragile roof controls and safe access are planned before work starts, not improvised on site.

Coating, overcladding or re-sheeting?

The sheet, the fixings and the insulation decide which of the three is honest.

Coating

Where sheets are structurally sound and the problem is laps, fixings, cut edges or a chalked factory finish.

Overcladding

Adds a new sheet above the old. It increases load and raises the roof line, and the existing roof stays in place underneath.

Re-sheeting

Where sheets are perforated, purlins have lost section or the roof needs to change thermally.

Failure modes

Why metal roofs fail at the details, not the field of the sheet

The middle of a metal sheet is usually sound. Failure concentrates at the edges and interfaces: cut edge corrosion creeping back from eaves and gutter line, fastener heads where the sealing washer has perished, laps where the original sealant has hardened, and flashings that have moved with thermal cycling.

Plastisol and similar factory coatings also chalk and thin under UV, which is a finish problem rather than a waterproofing one until the steel underneath starts to corrode. Understanding which of these is happening decides whether a coating, a repair or overcladding is the right answer.

  • Cut edge corrosion along eaves and gutter line
  • Perished sealing washers and backed-out fasteners
  • Failed lap sealant and open side laps
  • Chalked or thinning factory coatings
  • Thermal movement at flashings and ridge details
  • Condensation, which is not a coating defect at all

Options

Coating, overcladding or re-sheeting a metal roof

Coating suits a roof whose sheets are structurally sound and whose problem is water ingress at laps, fixings and edges. It adds almost no weight, needs no crane, and can be done in phases without an open roof.

Overcladding adds a new sheet above the old, which increases load, raises the roof line and usually requires the old roof to remain as a substrate. Re-sheeting is the right answer where sheets are perforated, purlins have lost section, or the roof needs to change thermally. Ask which one the survey supports before discussing price.

Preparation

On a metal roof, preparation is the specification

A coating is only as good as the bond beneath it. That means removing contamination, treating corrosion, dealing with loose factory coatings, priming where the system requires it, and checking adhesion before the full roof is sprayed.

This is the difference between a membrane and a paint. A decorative roof paint sits on the surface and follows every movement of the sheet until it cracks; a reinforced liquid rubber membrane is specified with the thickness and detailing to accommodate that movement.

Comfort

Condensation and solar gain are separate problems

If the complaint is dripping from the underside of a metal roof in cold weather, that is condensation, and a coating on the outside will not fix it. The remedy is ventilation, a vapour control layer or additional insulation, and it should be diagnosed at survey rather than discovered after the roof has been coated.

Solar gain is different again. A reflective finish can reduce surface temperature and thermal movement, and it is worth specifying on roofs with high solar exposure, but it is a performance addition rather than a waterproofing one.

Why liquid rubber suits a metal roof

A seamless membrane over a profiled, moving, heavily penetrated substrate: that is the engineering case for liquid rubber on steel.

Substrates
Galvanised steel, plastisol and coated profiles, aluminium
Profile
Spray application follows the profile, laps and ribs in one continuous layer
Membrane
2.0 mm seamless liquid rubber with reinforcement at details
Movement
Flexible cured membrane accommodates thermal movement of the sheet
Fire risk
Cold applied: no flame above combustible linings or stored goods
Minimum area
300 m² for spray application

What this page answers

The search terms this page covers, and the answer each one gets.

Search termIntentAnswer on this page
metal roof coatingCommercialA seamless membrane over prepared profiled steel
metal roof refurbishmentCommercialCoating, overcladding and re-sheeting compared
cut edge corrosion treatmentInformationalWhy corrosion starts at the eaves and gutter line
metal roof leaking at fixingsInformationalPerished washers and backed-out fasteners
metal roof condensationInformationalWhy a coating will not stop internal dripping

What drives the cost on a metal roof

The coating is rarely the largest item. Preparation, access and the condition of the sheets decide the number.

  • Measured area, profile and number of separate roof levels
  • Extent of corrosion, cut edge treatment and sheet replacement
  • Fixings, laps, rooflights, gutters and penetration details
  • Access: scaffold, MEWP, edge protection and fragile-roof controls
  • Working hours, waste, delivery and VAT

Warranty and handover

SprayGrade carries a 15-year system warranty and HBS200 a 25-year system warranty, subject to the exact specification, installation and written conditions. Confirm the proposed build-up, exclusions, inspection requirements and whether workmanship cover is separate before placing an order.

The programme

Allow for the complete job, not just application output. Preparation, access, curing and weather determine the agreed completion date.

  1. Survey and diagnose

    Measure the roof, identify materials and defects, and assess structure, moisture, fragility and drainage.

  2. Agree scope and access

    Confirm the system, preparation, repairs, access protection, work zones and site restrictions.

  3. Prepare and repair

    Use the preparation method appropriate to the material. Complete defect repairs and adhesion checks before coating.

  4. Detail and apply

    Treat junctions and apply the specified membrane at the required thickness, planned around weather windows.

  5. Inspect and hand over

    Record application checks, inspect details and drainage, and provide the agreed warranty and maintenance information.

Metal roof coating and refurbishment: questions answered

Can you coat a galvanised metal roof?

Yes, with correct preparation. Galvanised surfaces need cleaning and, depending on condition, a suitable primer to achieve adhesion. Adhesion is checked before the main application rather than assumed.

Does coating a metal roof stop rust?

It interrupts the corrosion cycle by sealing the surface and cut edges from water and oxygen. Existing corrosion has to be treated first, and sections that have corroded through cannot be rebuilt by a coating.

How long does a metal roof coating last?

The system is a 2.0 mm liquid rubber membrane with a 15 year system warranty available, subject to written terms. Life depends on preparation, specification and maintenance of gutters, outlets and details.

Can it be applied over plastisol coated sheeting?

Often yes, after assessment of the factory coating's condition and adhesion. Chalked or flaking plastisol needs preparation before any coating will bond reliably.

Will a coating stop condensation dripping inside the building?

No. Condensation is a thermal and ventilation issue on the underside of the sheet. It should be diagnosed separately, otherwise a perfectly good roof coating will not solve the complaint.

Is coating cheaper than overcladding?

Usually, and it adds no load to the structure. Overcladding becomes the better route where sheets are perforated or the roof needs to change thermally.

Specifications and related guidance

Discuss your roof

Send the postcode, approximate roof area, known covering, leak history and operating restrictions. Use existing photographs or drawings; do not access an unsafe roof to obtain them. Survey arrangements and timescales are confirmed with the team.

Contact the technical team